We update this knowledge base as we learn from our test lab and from your questions.
October 2026
- Launched the Pro PCTG knowledge base, built from our support team's most common answers.
- Pressure advance is now our top recommendation. See Pressure advance: why it matters.
- Snapmaker U1: disable automatic Extrusion Flow Calibration. See Snapmaker U1 notes.
- Updated drying recommendation: 70°C for 6–8 hours, or 65°C for 8–12 hours.
Comments