Skip to main content
Troubleshooting Updated

Bed Adhesion and Warping

John Schneider

PET-CF has very low warping, so most adhesion problems are easy to fix.

  • Use smooth or textured PEI. Wash it with hot water and dish soap before printing.
  • Bed temperature: 80–100°C. Go toward the top of the range for large parts.
  • Check the first layer. It should be slightly squished.
  • Use a brim on tall or narrow parts.

Was this article helpful?

0 out of 0 found this helpful
Have more questions? Submit a request

Comments

0 comments

Please sign in to leave a comment.