Stringing between parts of a print usually means the temperature is too high or retraction isn't long enough.
- Lower the nozzle temperature 5–10°C, staying within 230–250°C.
- Increase retraction by 1 mm at a time.
- Dry the filament. Wet filament strings more and gives a rougher surface. See Drying and storage.
- Test with a retraction test model. Search online for "retraction test model" to dial it in quickly.
Still stuck? Contact our support team with photos, your printer and nozzle, your slicer, and any changes you made to our profile.